Application In normal sulphate nickel plating bath, >20mg/L copper impurity can deteriorate the nickel deposit and cause blackening in LCD areas. Compared with low current electrolyzing or raising pH to subside, QT saves a lot of time and nickel. If adding QT 0.2-0.4g/L into bath once a month or ahead of treating nickel-plating bath, the problem of darkening or blackening caused by excessive copper impurity can be resolved. It's a stable, reliable, fast and effective way to maintain the stability of nickel-plating bath.
Storage Non-dangerous articles, be stored at cool and dry place
Concentration In Bath 0.1-0.2 g/L